The Iron-Carbon Phase Diagram: A Map of the Steel World

Release time:

2026-11-18

Author:

Source:


Summary

The iron-carbon phase diagram is a map that tells you, for any carbon content and temperature, exactly what structure a steel or cast iron will have. Four points — S at 727°C, C at 1148°C, E at 2.11% and P at 0.0218% — plus three key lines define every transformation.

The Iron-Carbon Phase Diagram: A Map of the Steel World

The iron-carbon phase diagram is a map that tells you, for any carbon content and temperature, exactly what structure a steel or cast iron will have. Four points — S at 727°C, C at 1148°C, E at 2.11% and P at 0.0218% — plus three key lines define every transformation.

1. How to read the diagram

The horizontal axis is carbon content (wt%, from 0 to 6.69%) and the vertical axis is temperature. Every line and intersection marks a phase transformation — a critical condition where atomic arrangement changes.

Note first: the diagram in common use is the metastable Fe-Fe₃C diagram (carbon as cementite); all heat treatment, quenching and annealing rely on it. A separate stable Fe-C diagram (carbon as graphite) is used mainly for cast iron.

2. The three basic phases

Ferrite F (α-Fe): body-centered cubic, very soft and tough, but dissolves almost no carbon — 0.0218% max at 727℃, only 0.0008% at room temperature — like soft clay. Austenite A (γ-Fe): face-centered cubic, exists only at high temperature, extremely ductile, dissolves up to 2.11% carbon — steel is forgeable only in this state, like warmed dough. Cementite Fe₃C: an iron-carbon compound with 6.69% carbon, extremely hard and brittle, like broken glass in dough — it supplies hardness.

3. Four critical points and three key lines

Four points (values per standard textbooks):

Point

Temp

Carbon

Meaning

S eutectoid

727°C

0.77%

Austenite decomposes into ferrite+cementite = pearlite; A1 temperature

C eutectic

1148°C

4.3%

Liquid crystallizes into austenite+cementite = ledeburite; best casting point

E

1148°C

2.11%

Max carbon solubility in austenite; steel/cast-iron boundary

P

727°C

0.0218%

Max carbon solubility in ferrite

 

Three lines: PSK (A1, 727°C) — all steels undergo eutectoid transformation to pearlite here. GS (A3) — temperature where hypoeutectoid steel begins to precipitate ferrite on cooling. ES (Acm) — line where hypereutectoid steel precipitates secondary cementite.

4. How carbon content changes microstructure

Reading the steel region from left to right:

Hypoeutectoid steel (0.0218–0.77%): room-temperature structure is ferrite + pearlite; more carbon means more pearlite and a harder steel. Eutectoid steel (0.77%): all pearlite, a good balance of strength and ductility. Hypereutectoid steel (0.77–2.11%): pearlite + secondary cementite; a network of cementite along grain boundaries is brittle, so tool steels need heat treatment to break it up.

In the cast-iron region (>2.11%), compositions near the C point (4.3%) have the lowest melting point and best fluidity, reproducing intricate mold details such as manhole-cover patterns. But high carbon means brittleness: machining only, never forging.

5. The three transformations of cementite

Fe₃C on the diagram often carries Roman numerals. Their chemistry is identical; only their origin differs:

Fe₃CⅠ (primary): crystallizes directly from liquid iron. Fe₃CⅡ (secondary): precipitates from austenite. Fe₃CⅢ (tertiary): precipitates from ferrite below 727℃, in negligible amounts.

Their morphology — coarse blocks, networks, fine particles — directly determines brittleness. This is why identical chemistry can yield wildly different properties after different heat treatments.

Next: Where does the carbon go? Interstitial solution and alloying elements.

Recommended reading


The Iron-Carbon Phase Diagram: A Map of the Steel World


The iron-carbon phase diagram is a map that tells you, for any carbon content and temperature, exactly what structure a steel or cast iron will have. Four points — S at 727°C, C at 1148°C, E at 2.11% and P at 0.0218% — plus three key lines define every transformation.

2026-11-18

The "DNA" of Metal: How Crystal Structures Determine Steel's Behavior


Metal atoms stack in three repeating patterns called crystal lattices — BCC, FCC and HCP — and this hidden order is the DNA that decides whether a metal is soft, tough or hard to machine. Real lattices always contain defects, and dislocations and grain boundaries are what actually control strength and ductility. Understanding them explains why stainless steel work-hardens and why grain refinement is the only way to raise strength and toughness at once. Bottom line: metal atoms are not piled randomly but arranged in fixed geometric patterns — crystal lattices. There are only three such patterns, yet they decide hardness, ductility and machinability. The lattice is a material's DNA.

2026-11-18

Steel vs. Cast Iron: What the 2.11% Carbon Threshold Really Means


Steel and cast iron are both iron-carbon alloys, separated by a single line: 2.11% carbon. Below it, carbon dissolves into iron's crystal lattice and the metal stays tough, forgeable and weldable. Above it, excess carbon precipitates as graphite, the metal turns brittle, and casting becomes the only forming route. Bottom line: Steel and cast iron are both iron-carbon alloys. The single dividing line is 2.11% carbon. Below it, carbon dissolves inside iron's crystal lattice and the metal can be forged and rolled. Above it, there is more carbon than the lattice can hold; the excess precipitates as graphite, the metal turns brittle, and casting becomes the only forming route.

2026-11-18

图片名称

Consultation



To provide you with high-quality products and services

Submit